Acier inoxydable, austénitique
317 Stainless Steel (S31700) Sheet & Plate
Une version modifiée de l'acier inoxydable de type 316 à haute résistance et résistance à la corrosion.
Type 317 is an austenitic chromium-nickel stainless steel with excellent corrosion resistance; Its high Molybdenum content enhances the grade’s superior pitting resistance. It was designed to be a higher strength alternative to the 316 grades.
Composed of larger amounts of chromium, nickel and molybdenum, alloy 317 also is more corrosion resistant compared to 316, and tougher than Type 304. This is the due to the high percentage of iron in its composition, which is much higher than many stainless steels.
This combination of iron with the chromium-nickel-molybdenum content yields a strong alloy.
It combines good mechanical properties, excellent weldability, and formability, ce qui en fait un choix idéal pour des applications dans chemical processing, marine environments, and industrial equipment where resistance to corrosion par piqûres, corrosion caverneuse et attaque chimique is essential.
TELECHARGER LE PDF
Gamme
Veuillez noter
Si vous ne voyez pas ce que vous cherchez, veuillez contacter votre Centre de services local avec vos exigences spécifiques.
317 Stainless Steel Related Specifications
| Système / Standard | Pays / Région | Grade / Désignation |
| AISI | ÉTATS-UNIS | 317 |
| Nations Unies | International | S31700 |
| FR / Numéro de dossier. | Europe | 1.4449 |
| EN Name (EN 10088) | Europe | X5CrNiMo18-15-4 |
| ASTM A240 | ÉTATS-UNIS | 317 (plate, sheet, strip) |
| ASTM A276 | ÉTATS-UNIS | 317 (bars, shapes) |
| ASTM A213 | ÉTATS-UNIS | TP317 (boiler / HX tubes) |
| ASTM A312 | ÉTATS-UNIS | TP317 (seamless pipe) |
| RU | Chine | 0Cr19Ni13Mo3 |
| ISJ | Japon | SUS317 |
| BS | Royaume-Uni | 317S16 |
| AFNOR | France | Z10CND19-15-04 |
Propriétés
Composition chimique
S31700 Sheet and Plate
ASTM A240
| Élément chimique | % Présent |
| Carbone (C) | 0.00 - 0.08 |
| Chrome (Cr) | 18.00 - 20.00 |
| Nickel (Ni) | 11.00 - 15.00 |
| Manganèse (Mn) | 0.00 - 2.00 |
| Phosphore (P) | 0.00 - 0.04 |
| Soufre (S) | 0.00 - 0.03 |
| Silicium (Si) | 0.00 - 0.75 |
| Molybdène (Mo) | 3.00 - 4.00 |
| Azote (N) | 0.00 - 0.10 |
| Fer (Fe) | Équilibre |
Propriétés mécaniques
ASTM A240
| Propriété mécanique | Valeur |
| Limite d'élasticité conventionnelle | 205 MPa |
| La résistance à la traction | 515 MPa |
| Allongement A50 mm | 35 Min % |
Applications of 317 Stainless Steel
317 stainless steel is an acier inoxydable austénitique avec high molybdenum content, offering enhanced corrosion resistance, especially in chemical, chloride, and oxidizing environments. It is widely used in applications that require durability, corrosion resistance, and good mechanical properties.
1. Industrie chimique et pétrochimique
Réacteurs, réservoirs et cuves pour produits chimiques corrosifs
Échangeurs de chaleur et condenseurs
Systèmes de tuyauterie manipulant des acides et des chlorures
Valves, pumps, and fittings in chemical processes
2. Marine Applications
Composants exposés à l'eau de mer ou à l'eau saumâtre
Tuyauterie marine et équipement structurel
Composants d'une usine de dessalement
3. Industrie alimentaire et pharmaceutique
Équipement de traitement nécessitant une résistance à la corrosion et une hygiène
Storage tanks, piping, and reactors for acidic or aggressive media
Échangeurs de chaleur, évaporateurs et agitateurs
4. Industrial Applications
Fasteners, bolts, and screws in aggressive environments
Structural components in chemical or industrial settings
Composants exposés à une forte humidité ou à des conditions salines
Résumé
317 stainless steel is widely used in applications chimiques, marines, pharmaceutiques et industrielles où une résistance supérieure à la corrosion, en particulier à chlorures et acides oxydants, est essentiel. Son austenitic structure, weldability, and durability la rendre idéale pour critical components exposed to harsh environments.
Characteristics of 317 Stainless Steel
317 stainless steel is an acier inoxydable austénitique avec enhanced corrosion resistance, mainly due to its high molybdenum content. It is widely used in environments that are more aggressive than those suitable for 316 stainless steel.
1. Résistance supérieure à la corrosion
Une teneur élevée en molybdène améliore la résistance à corrosion par piqûres et corrosion caverneuse, notamment en environnements contenant du chlorure.
Performe bien dans acides oxydants and moderately aggressive chemical solutions.
2. Structure austénitique
Fournit excellente ductilité, tenacité et formabilité.
Maintains mechanical properties at températures élevées et basses.
3. Propriétés Mécaniques
Bonne résistance à la traction, limite d'élasticité et allongement.
Peut résister stress and load in industrial applications without deformation.
4. Soudabilité et fabrication
Can be easily welded using TIG, MIG, and SMAW méthodes.
Low risk of sensibilisation due to controlled carbon content.
Suitable for forming into sheets, plates, piping, and complex components.
5. Applications liées aux caractéristiques
Chemical processing equipment
Marine equipment exposed to seawater
Pharmaceutical and food processing machinery
Heat exchangers, tanks, and industrial piping
Résumé
317 stainless steel is characterized by high corrosion resistance, good mechanical properties, excellent ductility, and reliable weldability. Son high molybdenum content makes it particularly suitable for applications chimiques, marines, pharmaceutiques et industrielles where aggressive environments are present.
Informations supplémentaires
Fabrication
Fabrication of 317 Stainless Steel
317 stainless steel is an austenitic, high-molybdenum stainless steel connu pour son excellente résistance à la corrosion and good mechanical properties. It can be fabricated using conventional techniques, including formation, soudage et usinage, making it suitable for industrial, chemical, and marine applications.
1. Formation
Travail à froid :
Suitable for bending, rolling, deep drawing, and stamping.
Work hardens moderately; recuit intermédiaire is recommended for extensive forming.
Travail à chaud :
Performed at elevated temperatures to reduce work hardening.
Plage de travail à chaud typique : 1150–900°C (2100–1650°F).
2. Soudage
Can be welded using standard techniques: TIG, MIG, SMAW et FCAW.
Métaux d'apport tels que ER317 or ER317L are recommended for maintaining corrosion resistance in welded joints.
Low risk of sensitization due to controlled carbon content, minimizing corrosion intergranulaire.
3. Usinage
Moderate machinability; work hardens during machining.
Utiliser outils en carbure tranchants, adequate feed, and proper coolant for optimal results.
Suitable for making piping, fittings, fasteners, and other precision components.
4. Traitements après fabrication
Recuit Restores ductility and relieves residual stresses after cold working or welding.
Décapage et passivation : Removes scale and restores the protective chromium oxide layer to optimize corrosion resistance.
5. Applications liées à la fabrication
Équipements de traitement chimique et pétrochimique
Composants exposés à la marine et à l'eau de mer
Machines pour le traitement des aliments et des produits pharmaceutiques
Tanks, piping systems, and industrial structural parts
Résumé
317 stainless steel is très fabricable, prenant en charge le formage à froid et à chaud, le soudage et l'usinage. Son high corrosion resistance, good mechanical properties, and weldability la rendre idéale pour applications chimiques, marines, pharmaceutiques et industrielles.
Soudabilité
Weldability of 317 Stainless Steel
317 stainless steel is an austenitic, high-molybdenum stainless steel avec excellente soudabilité, making it suitable for applications where corrosion-resistant welded components are required.
1. Soudabilité générale
Can be welded using all standard fusion welding techniques, including:
TIG (GTAW)
MIG (GMAW)
SMAW (Soudage à l'arc avec électrode enrobée)
Soudage à fil fourré
Welded joints maintain good corrosion resistance, mechanical strength, and toughness.
2. Low Carbon Content
Minimise sensibilisation lors du soudage.
Réduit le risque de corrosion intergranulaire, especially in welded zones.
Post-weld heat treatment is usually pas requis for maintaining corrosion resistance.
3. Recommandations sur le métal d'apport
Commonly used filler metals:
ER317 ou ER317L for matching corrosion resistance and mechanical properties
ER316L for less aggressive environments
Ensures consistent performance of welded joints.
4. Apport de chaleur et préparation
Un apport de chaleur modéré est recommandé pour éviter une croissance excessive du grain.
Ensure joint surfaces are clean, free of oil, grease, or oxide scale.
Preheating is generally not necessary.
5. Considérations post-soudage
Picklage ou passivation can be applied to restore the chromium oxide layer and optimize corrosion resistance.
Stress relief may be performed if the component is heavily stressed or exposed to high temperatures.
6. Applications liées à la soudabilité
Chemical processing tanks and piping
Composants exposés à la marine et à l'eau de mer
Food and pharmaceutical processing equipment
Heat exchangers, reactors, and industrial vessels
Résumé
317 stainless steel exhibits excellente soudabilité due to its austenitic structure and high molybdenum content. Proper filler selection and controlled welding techniques produce strong, corrosion-resistant joints, making 317 ideal for applications chimiques, marines, pharmaceutiques et industrielles.
Usinabilité
Machinability of 317 Stainless Steel
317 stainless steel is an austenitic, high-molybdenum stainless steel qui fournit usinabilité moyenne, similar to other austenitic stainless steels. Its combination of corrosion resistance and work-hardening characteristics requires careful machining practices.
1. Écrouissage
317 stainless steel le travail durcit rapidement, especially during light cuts or interrupted cuts.
To minimize work hardening:
Utiliser sharp, rigid tools
Avoid shallow cuts or repeated passes
Employ adequate lubrication and coolant
2. Recommandations d'outils
Outils en carbure are preferred for longer tool life and efficient cutting.
High-speed steel (HSS) tools can be used at lower cutting speeds.
Ensure rigid fixturing to reduce vibration and improve surface finish.
3. Conditions de coupe
Utiliser vitesses de coupe modérées à faibles to prevent overheating.
Maintain proper feed rate and depth of cut pour réduire le frottement de l'outil.
Continuous coolant flow helps with chip evacuation and tool cooling.
4. Formation des copeaux
Produit copeaux longs et ductiles en raison de sa structure austénitique.
Utiliser chip breakers or controlled cutting techniques pour gérer efficacement les jetons.
5. Finition de surface
Achievable with proper tooling and coolant.
Overheating during machining can degrade surface quality and reduce corrosion resistance.
6. Applications liées à l'usinage
Composants de précision en équipement chimique et pétrochimique
Fittings, valves, and fasteners for aggressive environments
Piping, tanks, and machinery requiring corrosion-resistant parts
Résumé
317 stainless steel exhibits usinabilité moyenne with a high work-hardening tendency. Using proper tooling, cutting speeds, and lubrication ensures efficient machining and excellent surface finish. Its combination of machinability and superior corrosion resistance le rend adapté à applications chimiques, marines, pharmaceutiques et industrielles.
Résistance à la corrosion
Corrosion Resistance of 317 Stainless Steel
317 stainless steel is an austenitic, high-molybdenum stainless steel qui fournit excellente résistance à la corrosion, particularly in aggressive environments containing chlorides, oxidizing acids, or other chemical media. Its higher molybdenum content compared to 316 stainless steel enhances resistance to corrosion par piqûres, corrosion caverneuse et attaque chimique.
1. Résistance générale à la corrosion
Résiste oxidation and general atmospheric corrosion.
Performe bien dans moderately aggressive chemical environments, y compris les acides doux et les solutions alcalines.
Convient à industrial and outdoor applications.
2. Corrosion par piqûres et corrosion caverneuse
Une teneur élevée en molybdène améliore la résistance à localized corrosion.
Particulièrement efficace en environnements riches en chlorures, comme l'eau de mer ou des solutions salines.
Outperforms 316 stainless steel in highly aggressive chemical or marine environments.
3. Résistance à la corrosion intergranulaire
Low carbon content minimizes the risk of sensibilisation lors du soudage.
Maintient la résistance à corrosion intergranulaire (CIG) in welded or heat-treated components.
4. Résistance à l'attaque chimique
Performe bien dans acides oxydants comme l'acide nitrique.
Fournit une résistance modérée à les acides réducteurs (par exemple, acide chlorhydrique) dans des conditions contrôlées.
Ideal for chemical reactors, tanks, and piping exposed to aggressive fluids.
5. Limites
Sous susceptible de stress corrosion cracking (SCC) in hot chloride solutions under high tensile stress.
May experience localized attack in strongly reducing or highly acidic environments.
6. Applications relatives à la résistance à la corrosion
Équipements de traitement chimique et pétrochimique
Composants exposés à la marine et à l'eau de mer
Machines pour le traitement des aliments et des produits pharmaceutiques
Échangeurs de chaleur, tuyauterie et réservoirs de stockage
Résumé
317 stainless steel provides excellente résistance globale à la corrosion, notamment dans environnements riches en chlorures et oxydants, thanks to its high molybdenum content. Its combination of résistance à la corrosion, soudabilité et formabilité en fait, il est idéal pour applications chimiques, marines, pharmaceutiques et industrielles.
Travail à froid
Cold Working of 317 Stainless Steel
317 stainless steel is an austenitic, high-molybdenum stainless steel avec bonne ductilité et formabilité, making it suitable for various cold working operations. Cold working increases strength through écrouissage while maintaining corrosion resistance.
1. Procédés de travail de base
Pliage et Formage : Peut être façonné en géométries complexes pour les réservoirs, la tuyauterie et les composants structurels.
Roulement : Produces sheets, strips, and coils.
Emboutissage Allows production of containers, trays, and intricate components.
Estampage et poinçonnage : Suitable for chemical, marine, and industrial applications.
2. Durcissement par travail
317 stainless steel le travail durcit rapidement, augmentant la résistance à la traction et à la limite d'élasticité pendant la déformation.
Un travail à froid excessif peut réduire la ductilité.
Recuit intermédiaire est recommandé pour le formage intensif afin de restaurer la ductilité et de soulager les contraintes internes.
3. Considérations relatives à la fabrication
Appliquer déformation progressive pour éviter de fissurer ou de surmener le matériau.
Use proper tooling, lubrication, and support to maintain surface finish and dimensional accuracy.
Les composants travaillés à froid peuvent nécessiter soulagement du stress pour les applications critiques.
4. Applications liées à l'usinage à froid
Équipements de traitement chimique et pétrochimique
Composants marins exposés à l'eau de mer
Machines pour le traitement des aliments et des produits pharmaceutiques
Réservoirs, tuyauteries et pièces de structure nécessitant une résistance à la corrosion
Résumé
317 stainless steel exhibits excellentes caractéristiques de déformation à froid, permettant le pliage, le cintrage, le matriçage et l'emboutissage. Le travail à froid améliore la résistance tout en maintenant résistance à la corrosion, ce qui le rend idéal pour applications chimiques, marines, pharmaceutiques et industrielles.
Traitement thermique
Heat Treatment of 317 Stainless Steel
317 stainless steel is an austenitic, high-molybdenum stainless steel. Like other austenitic stainless steels, it is non trempable par traitement thermique conventionnel. Le traitement thermique est principalement utilisé pour restore ductility, relieve stresses, and optimize corrosion resistance after fabrication or cold working.
1. Recuit
Purpose: Restore ductility, relieve stresses, and enhance corrosion resistance after cold working or welding.
Annealing temperature: 1040–1120°C (1900–2050°F)
Refroidissement Rapid cooling in air or water to maintain corrosion resistance and prevent sensitization.
2. Gestion du stress
Applied to reduce residual stresses from cold working, welding, or machining.
Gamme de température : 450–650 °C (840–1200 °F)
Helps improve stabilité dimensionnelle and reduces the risk of stress-related cracking.
3. Effets du traitement thermique
Restores ductility and toughness in cold-worked areas.
Élimine les contraintes résiduelles de soudage ou de fabrication.
Est-ce que not increase strength significantly, as 317 is not precipitation-hardenable.
4. Surface Treatment Post Heat
Picklage ou passivation may be applied after heat treatment to remove scale or oxides and restore the protective chromium oxide layer.
5. Applications liées au traitement thermique
Tuyauterie, réservoirs et récipients soudés dans le traitement chimique
Heat exchangers, reactors, and high-temperature equipment
Marine and pharmaceutical equipment exposed to heat
Résumé
Heat treatment of 317 stainless steel is mainly for Recuit et détente des contraintes, en maintenant ductilité, résistance à la corrosion et stabilité dimensionnelle. This ensures reliable performance in applications chimiques, marines, pharmaceutiques et industrielles, particularly after fabrication or welding.
Résistance à la chaleur
Heat Resistance of 317 Stainless Steel
317 stainless steel is an austenitic, high-molybdenum stainless steel avec une bonne résistance à oxydation et écaillement à haute température. Its composition allows it to maintain mechanical integrity and corrosion resistance in moderately high-temperature environments.
1. Température de service continue
Convient à continuous use up to approximately 870°C (1600°F) dans des atmosphères oxydantes.
Maintient mechanical strength and corrosion resistance under sustained heat exposure.
2. Exposition intermittente
Peut résister expositions de courte durée ou intermittentes jusqu'à 925°C (1700°F) sans mise à l'échelle ou oxydation significative.
Adapté aux composants exposés à cyclage thermique ou des températures élevées fluctuantes.
3. Résistance à l'oxydation
Forme un stable couche d'oxyde de chrome qui protège contre le tartre et l'oxydation.
High molybdenum content enhances resistance to localized attack during high-temperature exposure.
4. Limites
Ne convient pas à un service prolongé à des températures extrêmement élevées (>925°C / 1700°F).
Sous susceptible de stress corrosion cracking dans des environnements chauds contenant des chlorures.
5. Applications liées à la résistance à la chaleur
Échangeurs de chaleur, chaudières et composants de four dans les industries chimique et pétrochimique
Tuyauterie et réservoirs haute température
Matériel marin exposé à des températures élevées
Équipement industriel nécessitant une résistance modérée à la chaleur combinée à une résistance à la corrosion
Résumé
317 stainless steel provides bonne résistance à la chaleur pour service continu jusqu'à 870°C et une exposition intermittente jusqu'à 925°C, tout en conservant une résistance à la corrosion et une intégrité mécanique. Sa combinaison de résistance à la chaleur, résistance à la corrosion et soudabilité le rend adapté à applications chimiques, marines, pharmaceutiques et industrielles.
Travail à chaud
Hot Working of 317 Stainless Steel
317 stainless steel is an austenitic, high-molybdenum stainless steel avec de bonnes travail à chaud. Hot working allows shaping and forming at elevated temperatures while minimizing work hardening and maintaining mechanical and corrosion-resistant properties.
1. Température de travail à chaud
Plage de travail à chaud recommandée : 1150–900°C (2100–1650°F).
Un contrôle adéquat de la température empêche croissance du grain and preserves corrosion resistance and mechanical integrity.
2. Procédés de travail à chaud
Laminage à chaud : Produit des tôles, des plaques et des bandes d'épaisseur uniforme.
Forgeage Convient aux composants structurels et aux pièces haute température.
Extrusion : Permet la production de barres, tubes et profilés.
Pressage et Formage à Chaud : Utile pour façonner des géométries complexes avec un minimum de risque de fissuration.
3. Avantages du travail à chaud
Réduit écrouissage comparé à l'usinage à froid.
Améliore ductilité et ténacité dans le composant fini.
Facilitates production of grandes, épaisses ou complexes piÈces.
4. Traitements post-forge
Recuit peuvent être appliquées pour restaurer des propriétés mécaniques uniformes et soulager les contraintes résiduelles.
Picklage ou passivation améliore la résistance à la corrosion de surface après un travail à chaud.
5. Applications liées au travail à chaud
Échangeurs de chaleur, composants de fournaise et tuyauterie à haute température
Composants structurels pour équipements pétrochimiques et de production d'énergie
Pièces industrielles nécessitant des performances à haute température et une résistance à la corrosion
Résumé
317 stainless steel exhibits excellentes caractéristiques de travail à chaud, permettant le laminage, le forgeage, l'extrusion et le formage complexe à 1150–900°C. Le travail à chaud réduit l'écrouissage, améliore la ductilité et permet la production de pièces pour applications chimiques, marines, pharmaceutiques et industrielles à haute température.